Fig. 1 Shaping the tip of a monosteel blade with hammer and tongs.
Fig. 2 A soak in kerosene helps the steel heat to forge welding temperature quickly.
Fig. 3 Readying a stack of 1084 and 15n20 high carbon steel to be forged into Damascus steel.